____________ is a form of environmental cracking that can initiate on the surface of high strength low alloy steels and carbon steels with highly localized zones of high hardness in the weld metal and HAZ as a result of exposure to aqueous HF acid service.
A) Sulfide stress cracking
B) Hydrogen stress cracking
C) Caustic stress cracking
D) Hydrogen induced cracking
Correct Answer:
Verified
Q85: Corrosion of the anode may be significantly
Q86: _ corrosion rates are found in a
Q87: All _ based materials and low alloy
Q88: Damage from sigma phase appears in the
Q89: Alloys with nickel content above _ are
Q91: Sulfuric acid promotes general and localized corrosion
Q92: The extent and depth of decarburization is
Q93: With CO₂ corrosion, increasing temperatures _ corrosion
Q94: Which of these materials are susceptible to
Q95: HCL acid corrosion is found in several
Unlock this Answer For Free Now!
View this answer and more for free by performing one of the following actions
Scan the QR code to install the App and get 2 free unlocks
Unlock quizzes for free by uploading documents