Deck 30: Testing and Inspecting Welds

Full screen (f)
exit full mode
Question
Unless care is taken in reading radiographs, the presence of slag inclusions can be interpreted as other defects.
Use Space or
up arrow
down arrow
to flip the card.
Question
A discontinuity becomes a defect when the discontinuity becomes so large or when there are so many small discontinuities that the weld is not acceptable under the standards for the code for that product.
Question
____ occurs when the depth that the weld penetrates the joint is less than that needed to fuse through the plate or into the preceding weld.

A) Inclusions
B) Porosity
C) Incomplete fusions
D) Inadequate joint penetration
Question
To prevent undercutting, you can weld in the flat position by using multiple instead of single passes, change the shield gas, and improve manipulative techniques to fill the removed base metal along the toe of the weld bead.
Question
____ is the result of the arc force removing metal from a joint face that is not replaced by weld metal.

A) Crater crack
B) Incomplete fusion
C) Undercut
D) Overlap
Question
____ results from gas that was dissolved in the molten weld pool, forming bubbles that are trapped as the metal cools to become solid.

A) Inclusions
B) Porosity
C) Undercutting
D) Incomplete fusion
Question
____ inspection is a method for detecting flaws inside weldments.

A) Magnetic particle
B) Penetrant
C) Visual
D) Radiographic
Question
One common test used to determine the impact capability of a weld is the ____ test in which a notched specimen is struck by an anvil mounted on a pendulum.

A) Izod
B) Charpy
C) Fillet weld break
D) Free-bend
Question
The majority of welds receive only visual inspection.
Question
____ occurs in fusion welds when weld deposits are larger than the joint is conditioned to accept.

A) Overlap
B) Inclusion
C) Incomplete fusion
D) Arc strike
Question
____ porosity is most often caused by improper starting and stopping techniques.

A) Clustered
B) Linear
C) Piping
D) Uniformly scattered
Question
Although not visible, the development of inclusions can be expected if prior welds were improperly cleaned or had a poor contour.
Question
Tensile testing is used to determine how well a weld can resist repeated fluctuating stresses or cyclic loading.
Question
____ on a groove weld appears when the weld metal deposited is inadequate to bring the weld's face or root surfaces to a level equal to that of the original plane or plate surface.

A) Overlap
B) Underfill
C) Undercut
D) Inclusion
Question
____ inspection is used to locate minute surface cracks and porosity.

A) Visual
B) Magnetic particle
C) Penetrant
D) Radiographic
Question
Many acceptable products may have welds that contain defects. But no products may have welds that contain discontinuities.
Question
Lamellar tears differ from lamination because they are more extensive and involve thicker layers of nonmetallic contaminants.
Question
The three methods of testing welded butt joints are (1) the nick-break test, (2) the guided-bend test, and (3) the free-bend test.
Question
____ is the lack of coalescence between the molten filler metal and previously deposited filler metal and/or the base metal.

A) Inclusion
B) Crater crack
C) Inadequate joint penetration
D) Incomplete fusion
Question
Ultrasonic inspection (UT) is a nondestructive test. This method is based upon magnetic induction in which a magnetic field induces eddy currents within the material being tested.
Question
____________________ methods, except for hydrostatic testing, result in the product being destroyed.
Question
The difference between what is acceptable, fit for service, and perfection is known as ____________________.
Question
A lack of fusion between the filler metal and previously deposited weld metal is called ____________________.
Question
A cylindrical porosity is called a(n) ____________________, and it is the most likely type of porosity to reach the weld surface and be seen.
Question
____________________ inspection uses finely divided ferromagnetic particles (powder) to indicate defects open to the surface or just below the surface on magnetic materials.
Unlock Deck
Sign up to unlock the cards in this deck!
Unlock Deck
Unlock Deck
1/25
auto play flashcards
Play
simple tutorial
Full screen (f)
exit full mode
Deck 30: Testing and Inspecting Welds
1
Unless care is taken in reading radiographs, the presence of slag inclusions can be interpreted as other defects.
True
2
A discontinuity becomes a defect when the discontinuity becomes so large or when there are so many small discontinuities that the weld is not acceptable under the standards for the code for that product.
True
3
____ occurs when the depth that the weld penetrates the joint is less than that needed to fuse through the plate or into the preceding weld.

A) Inclusions
B) Porosity
C) Incomplete fusions
D) Inadequate joint penetration
D
4
To prevent undercutting, you can weld in the flat position by using multiple instead of single passes, change the shield gas, and improve manipulative techniques to fill the removed base metal along the toe of the weld bead.
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
5
____ is the result of the arc force removing metal from a joint face that is not replaced by weld metal.

A) Crater crack
B) Incomplete fusion
C) Undercut
D) Overlap
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
6
____ results from gas that was dissolved in the molten weld pool, forming bubbles that are trapped as the metal cools to become solid.

A) Inclusions
B) Porosity
C) Undercutting
D) Incomplete fusion
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
7
____ inspection is a method for detecting flaws inside weldments.

A) Magnetic particle
B) Penetrant
C) Visual
D) Radiographic
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
8
One common test used to determine the impact capability of a weld is the ____ test in which a notched specimen is struck by an anvil mounted on a pendulum.

A) Izod
B) Charpy
C) Fillet weld break
D) Free-bend
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
9
The majority of welds receive only visual inspection.
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
10
____ occurs in fusion welds when weld deposits are larger than the joint is conditioned to accept.

A) Overlap
B) Inclusion
C) Incomplete fusion
D) Arc strike
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
11
____ porosity is most often caused by improper starting and stopping techniques.

A) Clustered
B) Linear
C) Piping
D) Uniformly scattered
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
12
Although not visible, the development of inclusions can be expected if prior welds were improperly cleaned or had a poor contour.
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
13
Tensile testing is used to determine how well a weld can resist repeated fluctuating stresses or cyclic loading.
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
14
____ on a groove weld appears when the weld metal deposited is inadequate to bring the weld's face or root surfaces to a level equal to that of the original plane or plate surface.

A) Overlap
B) Underfill
C) Undercut
D) Inclusion
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
15
____ inspection is used to locate minute surface cracks and porosity.

A) Visual
B) Magnetic particle
C) Penetrant
D) Radiographic
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
16
Many acceptable products may have welds that contain defects. But no products may have welds that contain discontinuities.
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
17
Lamellar tears differ from lamination because they are more extensive and involve thicker layers of nonmetallic contaminants.
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
18
The three methods of testing welded butt joints are (1) the nick-break test, (2) the guided-bend test, and (3) the free-bend test.
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
19
____ is the lack of coalescence between the molten filler metal and previously deposited filler metal and/or the base metal.

A) Inclusion
B) Crater crack
C) Inadequate joint penetration
D) Incomplete fusion
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
20
Ultrasonic inspection (UT) is a nondestructive test. This method is based upon magnetic induction in which a magnetic field induces eddy currents within the material being tested.
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
21
____________________ methods, except for hydrostatic testing, result in the product being destroyed.
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
22
The difference between what is acceptable, fit for service, and perfection is known as ____________________.
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
23
A lack of fusion between the filler metal and previously deposited weld metal is called ____________________.
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
24
A cylindrical porosity is called a(n) ____________________, and it is the most likely type of porosity to reach the weld surface and be seen.
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
25
____________________ inspection uses finely divided ferromagnetic particles (powder) to indicate defects open to the surface or just below the surface on magnetic materials.
Unlock Deck
Unlock for access to all 25 flashcards in this deck.
Unlock Deck
k this deck
locked card icon
Unlock Deck
Unlock for access to all 25 flashcards in this deck.